단순화한 연소법에 의해 합성한 LiMn1.92Co0.08O4와 LiNi0.7Co0.3O2 혼합물의 전기화학적 특성
송명엽, 권익현, 김훈욱
전북대학교 신소재공학부 공학연구원 신소재개발연구센터
Electrochemical Properties of LiMn1.92Co0.08O4 and LiNi0.7Co0.3O2 Mixtures Prepared by a Simplified Combustion Method
Myoungyoup Song, IkHyun Kwon, Hunuk Kim
Division of Advanced Materials Engineering, Research Center of Advanced Materials Development. Engineering Research Institute, Chonbuk National University
ABSTRACT
$LiMn_{1.92}Co_{0.08}O_4$ and $LiNi_{0.7}Co_{0.3}O_2$ synthesized by a simplified combustion method had good electrochemical properties. Mixtures $LiMn_{1.92}Co_{0.08}O_4$-x wt$%$ $LiNi_{0.7}Co_{0.3}O_2$ (x=9, 23, 33, 41, and 47) were prepared by milling for 30 min and their electrochemical properties were investigated. The electrode with x=9 had a relatively large first discharge capacity (109.9 mAh/g at 0.1 C) and good cycling performance. The decrease in the discharge capacity of the mixture electrodes with cycling is considered to result mainly from the degradation of $LiNi_{0.7}Co_{0.3}O_2$, caused by coating of $LiNi_{0.7}Co_{0.3}O_2$ with Mn dissolved from $LiMn_{1.92}Co_{0.08}O_4$.
Key words: A Simplified combustion method, Mixture electrodes, First discharge Capacity, Cycling performance
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI