J. Korean Ceram. Soc. > Volume 32(3); 1995 > Article
Journal of the Korean Ceramic Society 1995;32(3): 378.
$La_2O_3$$MnO_2$$0.02Pb(Y_{2/3}W_{1/3}O_3-0.98Pb(Zr_{0.52}Ti_{0.48})O_3$의 유전 및 압전 특성에 미치는 영향
윤석진, 류소연, 문종하1, 김현재, 오상록2, 이종원3, 정형진4
한국과학기술연구원 세라믹스 연구부
1전남대학교 무기재료공학과
2한국과학기술연구원 기전 연구부
3한국과학기술원 기전 연구부
4한국과학기술원 세라믹스 연구부
Effects of $La_2O_3$, $MnO_2$ on the Dielectric and Piezoelectric Properties of $0.02Pb(Y_{2/3}W_{1/3}O_3-0.98Pb(Zr_{0.52}Ti_{0.48})O_3$
ABSTRACT
Effects of $La_2O_3$, $MnO_2$ on the dielectric and piezoelectric properties of $0.02Pb(Y_{2/3}W_{1/3}O_3-0.98Pb(Zr_{0.52}Ti_{0.48})O_3$ system were investigated. The addition of La2O3 to the system enhanced electromechanical coupling factor (kp), piezoelectric constant (d33), but hardly changed mechanical quality factor (Qm). On the other hand, the addition of $MnO_2$ increased Qm significantly, but did not degrade kp and d33 so much. The piezoelectric properties of $0.02Pb(Y_{2/3}W_{1/3}O_3-0.98Pb(Zr_{0.52}Ti_{0.48})O_3$ containing 0.1wt% $La_2O_3$, 0.4wt% $MnO_2$ were very good and kp, d33, Qm were 55%, 350$times$10-12C/N, 780, respectively. The size of the grains was proportional to the change of c/a (tetragonality) ratio caused by the addition of $La_2O_3$ and $MnO_2$, and dielectric, piezoelectric properties were sensitive to the amountof pyrochrole phase.
Key words: $0.02Pb(Y_{2/3}W_{1/3}O_3-0.98Pb(Zr_{0.52}Ti_{0.48})O_3$, $MnO_2$, Electromechanical coupling factor (kp), Piezoelectric constant (d33), Mechanical quality factor (Qm), Tetragonality, Pyrochrole phase
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI