WC-Co의 열충격 후 파괴 현상과 기계적 성질
Fracture Behavior and Mechanical properties of WC-Co Subjected to Thermal Shock
한동빈 , Joh 1
Department of Materials Science and Engineering Pensylvania State University
1University of Florida
ABSTRACT
WC-Co composites are widely used as cutting or drilling tools because of their high hardness, strength, and fracture toughness. The working temperature is, however, generally in the range of 300-$700^{circ}C$ so thermal shock fracture of WC-Co can occur. In this study, the strength, fracture toughness and fracture surface of 16wt% Co bonded tungsten carbide composites before and after thermal shock were observed.
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI