ABSTRACT
$BaTiO_3$ and $SrTiO_3$ were mixed with the mole ratio of 35:65, 50:50 and 65:35 and heated at 1100~120$0^{circ}C$ for 1~64 hours. The dielectrics of $BaTiO_3$-$SrTiO_3$ system were investigated as a function of amount of solid solution formed. The dielectric constant was increased and Curie temperature was shifted to higher temperature with increasing of heating of soaking time for the same composition and heating temperature. This can be explained by the homogeneous distribution of $Ba^{2+}$ and $Sr^{2+}$ ion in the $BaTiO_3$ system. The Curie temperature was shifted to lower temperature with increasing $SrTiO_3$ in the $BaTiO_3$-$SrTiO_3$system because of decreasing the lattice constant.
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI