Defect Structure and Electrical Conductivity of Gadolinium Sesquioxide
ABSTRACT
The electrical conductivity of polycrystalline $Gd_2O_3$ has been measured over the temperature range of 650 to 100$0^{circ}C$ under the oxygen pressure range of $10^{-6}$ to 102 torr. The oxygen pressure dependence of electrical conductivity, $sigma$ PO211/n is characterized by n value of about 5.3. The defect structure and the type of the oxide are controlled by triply ionized metal vacancies and holes.
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI