ABSTRACT
This study is aimed at synthsizing high dielectric material (Ba, Sr)$TiO_3$ through direct wet process. Pure and ultra fine particle of (Ba, Sr)$TiO_3$ Powder was synthesized from $BaCl_2$ $SrCl_2$ and TiCl4 aqeous solution at KOH Solution in the $N_2$ gas atmosphere. $BaCl_2$ $SrCl_2$ and TiCl4 were Mixed with the mole ratio of 1:9, 3:7:10, 5:5:10, 7:3:10, 9:1:10 and sythesized at 4$0^{circ}C$~9$0^{circ}C$ for 10min~15hrs. The particle size particle shape crystallinity and synthesis condition of (Ba, Sr)$TiO_3$ powder with the variation of temperature and reaction time in the aqueous solution studied by the exprimental instruments of DTA. TGA, X-ray diffratometer SEM.
Editorial Office
Meorijae Bldg., Suite # 403, 76, Bangbae-ro, Seocho-gu, Seoul 06704, Korea
TEL: +82-2-584-0185   FAX: +82-2-586-4582   E-mail: ceramic@kcers.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Ceramic Society.                      Developed in M2PI